Materials with additional impregnation of pyrocarbon, resins, etc.
Name | Units | Range / value |
---|---|---|
Bulk Density | g/cm3 | 1,82 |
Compressive Strength | Mpa, at least | 200 |
Bending Strength | Mpa, at least | 75 |
Ash content | %, not more | On request |
Resistance | μΩM, not more | On request |
Average grain size | um, not more | On request |
Name | Units | Range / value |
---|---|---|
Bulk Density | g/cm3 | 2,25 |
Compressive Strength | Mpa, at least | 260 |
Bending Strength | Mpa, at least | 95 |
Ash content | %, not more | On request |
Resistance | μΩM, not more | On request |
Average grain size | um, not more | On request |
Name | Units | Range / value |
---|---|---|
Bulk Density | g/cm3 | |
Compressive Strength | Mpa, at least | |
Bending Strength | Mpa, at least | |
Ash content | %, not more | |
Resistance | μΩM, not more | |
Average grain size | um, not more |
Name | Units | Range / value |
---|---|---|
Bulk Density | g/cm3 | |
Compressive Strength | Mpa, at least | |
Bending Strength | Mpa, at least | |
Ash content | %, not more | |
Resistance | μΩM, not more | |
Average grain size | um, not more |
Name | Units | Range / value |
---|---|---|
Bulk Density | g/cm3 | |
Compressive Strength | Mpa, at least | |
Bending Strength | Mpa, at least | |
Ash content | %, not more | |
Resistance | μΩM, not more | |
Average grain size | um, not more |
№ | Trade name | Normative document | Characteristics |
---|---|---|---|
1 | EK2200 | On request | view properties |
2 | EK3205 | On request | view properties |
3 | АГ-1500 Б83 | On request | view properties |
4 | АТГ-Э | On request | view properties |
5 | Вар-253у | On request | view properties |