Name | Units | Range / value |
---|---|---|
Bulk Density | g/cm3 | 1,82 |
Compressive Strength | Mpa, at least | 200 |
Bending Strength | Mpa, at least | 75 |
Ash content | %, not more | On request |
Resistance | μΩM, not more | On request |
Average grain size | um, not more | On request |
Name | Units | Range / value |
---|---|---|
Bulk Density | g/cm3 | 2,25 |
Compressive Strength | Mpa, at least | 260 |
Bending Strength | Mpa, at least | 95 |
Ash content | %, not more | On request |
Resistance | μΩM, not more | On request |
Average grain size | um, not more | On request |
Name | Units | Range / value |
---|---|---|
Bulk Density | g/cm3 | On request |
Compressive Strength | Mpa, at least | On request |
Bending Strength | Mpa, at least | On request |
Ash content | %, not more | On request |
Resistance | μΩM, not more | On request |
Average grain size | um, not more | On request |
Name | Units | Range / value |
---|---|---|
Bulk Density | g/cm3 | 1,72 |
Compressive Strength | Mpa, at least | 30 |
Bending Strength | Mpa, at least | 14 |
Ash content | %, not more | 0,3 |
Resistance | μΩM, not more | 8 |
Average grain size | um, not more | - |
Name | Units | Range / value |
---|---|---|
Bulk Density | g/cm3 | |
Compressive Strength | Mpa, at least | |
Bending Strength | Mpa, at least | |
Ash content | %, not more | |
Resistance | μΩM, not more | |
Average grain size | um, not more |
Name | Units | Range / value |
---|---|---|
Bulk Density | g/cm3 | |
Compressive Strength | Mpa, at least | |
Bending Strength | Mpa, at least | |
Ash content | %, not more | |
Resistance | μΩM, not more | |
Average grain size | um, not more |
Name | Units | Range / value |
---|---|---|
Bulk Density | g/cm3 | 1,68 |
Compressive Strength | Mpa, at least | 30 |
Bending Strength | Mpa, at least | 14 |
Ash content | %, not more | 0,3 |
Resistance | μΩM, not more | 9 |
Average grain size | um, not more | 2 |
Name | Units | Range / value |
---|---|---|
Bulk Density | g/cm3 | |
Compressive Strength | Mpa, at least | |
Bending Strength | Mpa, at least | |
Ash content | %, not more | |
Resistance | μΩM, not more | |
Average grain size | um, not more |
Name | Units | Range / value |
---|---|---|
Bulk Density | g/cm3 | 1,77 |
Compressive Strength | Mpa, at least | 60 |
Bending Strength | Mpa, at least | 28 |
Ash content | %, not more | 0,1 |
Resistance | μΩM, not more | 9?12 |
Average grain size | um, not more | - |
Name | Units | Range / value |
---|---|---|
Bulk Density | g/cm3 | 1,7 |
Compressive Strength | Mpa, at least | 30 |
Bending Strength | Mpa, at least | 14 |
Ash content | %, not more | 0,01 |
Resistance | μΩM, not more | 9?12 |
Average grain size | um, not more | - |
Name | Units | Range / value |
---|---|---|
Bulk Density | g/cm3 | 1,83 |
Compressive Strength | Mpa, at least | 85 |
Bending Strength | Mpa, at least | 40 |
Ash content | %, not more | 0,1 |
Resistance | μΩM, not more | 9?12 |
Average grain size | um, not more | - |
Name | Units | Range / value |
---|---|---|
Bulk Density | g/cm3 | 1,85 |
Compressive Strength | Mpa, at least | 110 |
Bending Strength | Mpa, at least | 50 |
Ash content | %, not more | 0,1 |
Resistance | μΩM, not more | 9?12 |
Average grain size | um, not more | - |
Name | Units | Range / value |
---|---|---|
Bulk Density | g/cm3 | 1,8 |
Compressive Strength | Mpa, at least | 115 |
Bending Strength | Mpa, at least | 50 |
Ash content | %, not more | 0,05 |
Resistance | μΩM, not more | 13 |
Average grain size | um, not more | 0,02 |
Name | Units | Range / value |
---|---|---|
Bulk Density | g/cm3 | 1,83 |
Compressive Strength | Mpa, at least | 125 |
Bending Strength | Mpa, at least | 60 |
Ash content | %, not more | 0,02 |
Resistance | μΩM, not more | 13 |
Average grain size | um, not more |
Name | Units | Range / value |
---|---|---|
Bulk Density | g/cm3 | 1,85 |
Compressive Strength | Mpa, at least | 148 |
Bending Strength | Mpa, at least | 78 |
Ash content | %, not more | 0,1 |
Resistance | μΩM, not more | 18 |
Average grain size | um, not more | 0,02 |
Name | Units | Range / value |
---|---|---|
Bulk Density | g/cm3 | 1,6 |
Compressive Strength | Mpa, at least | 22 |
Bending Strength | Mpa, at least | 11 |
Ash content | %, not more | 0,3 |
Resistance | μΩM, not more | 8 |
Average grain size | um, not more | - |
Name | Units | Range / value |
---|---|---|
Bulk Density | g/cm3 | 1,65 |
Compressive Strength | Mpa, at least | 24 |
Bending Strength | Mpa, at least | 12 |
Ash content | %, not more | 0,3 |
Resistance | μΩM, not more | 7,5 |
Average grain size | um, not more | - |
№ | Trade name | Normative document | Characteristics |
---|---|---|---|
1 | EK2200 | On request | view properties |
2 | EK3205 | On request | view properties |
3 | Graphite felts | On request | view properties |
4 | А-22 | ТУ-1915-001-48534975-2014 | view properties |
5 | АГ-1500 Б83 | On request | view properties |
6 | АТГ-Э | On request | view properties |
7 | В-12 | ТУ-1915-001-48534975-2014 | view properties |
8 | Вар-253у | On request | view properties |
9 | Л-7 | ТУ-1915-001-48534975-2014 | view properties |
10 | Л-70 | ТУ-1915-001-48534975-2014 | view properties |
11 | Л-80 | ТУ-1915-001-48534975-2014 | view properties |
12 | Л-85 | ТУ-1915-001-48534975-2014 | view properties |
13 | С-4 | ТУ-1915-001-48534975-2014 | view properties |
14 | С-500 | ТУ-1915-001-48534975-2014 | view properties |
15 | С-7 | ТУ-1915-001-48534975-2014 | view properties |
16 | ЭГ | ТУ-1915-001-48534975-2014 | view properties |
17 | ЭГП | ТУ-1915-001-48534975-2014 | view properties |